The failure mode of natural silk epoxy triggered composite tubes

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Abstract

In this study the quasi static compression test over natural silk epoxy triggered composite tubes has been carried out, the natural silk epoxy composite tubes consist of 24 layer of woven natural silk as reinforcement and thermoset epoxy resin as matrix which both of them i e natural silk and epoxy have excellent mechanical properties More over the natural silk have better moisture resistance in comparison with other natural reinforcements, the length of tubes are 50, 80 and 120 mm The natural silk epoxy composite tubes are associated with an external trigger which includes 4 steel pieces welded on downside flat plate fixture The hand lay up fabrication method has been used to make the natural silk epoxy composite tubes Instron universal testing machine with 250 KN load capacity has been employed to accomplish this investigation The failure modes of natural silk epoxy triggered composite tubes has been investigated by representative photographs which has been taken by a high resolution camera(12 2 Mp) during the quasi static compression test, from the photographs is observed the failure modes is progressive local buckling

Original languageEnglish
Title of host publicationIOP Conference Series: Materials Science and Engineering
Volume36
Edition1
DOIs
Publication statusPublished - 2012
Event1st International Conference on Mechanical Engineering Research 2011, ICMER 2011 - Kuantan, Pahang, Malaysia
Duration: 5 Dec 20117 Dec 2011

Other

Other1st International Conference on Mechanical Engineering Research 2011, ICMER 2011
CountryMalaysia
CityKuantan, Pahang
Period5/12/117/12/11

Fingerprint

Silk
Failure modes
Composite materials
Reinforcement
Epoxy Resins
Steel
Thermosets
Epoxy resins
Buckling
Compaction
Moisture
Cameras
Fabrication
Mechanical properties
Testing

ASJC Scopus subject areas

  • Materials Science(all)
  • Engineering(all)

Cite this

Eshkour, R. A., Mohd Ihsan, A. K. A., Zulkifli, R., Sulong, A. B., & Azhari, C. H. (2012). The failure mode of natural silk epoxy triggered composite tubes. In IOP Conference Series: Materials Science and Engineering (1 ed., Vol. 36). [012030] https://doi.org/10.1088/1757-899X/36/1/012030

The failure mode of natural silk epoxy triggered composite tubes. / Eshkour, R. A.; Mohd Ihsan, Ahmad Kamal Ariffin; Zulkifli, Rozli; Sulong, Abu Bakar; Azhari, Che Husna.

IOP Conference Series: Materials Science and Engineering. Vol. 36 1. ed. 2012. 012030.

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Eshkour, RA, Mohd Ihsan, AKA, Zulkifli, R, Sulong, AB & Azhari, CH 2012, The failure mode of natural silk epoxy triggered composite tubes. in IOP Conference Series: Materials Science and Engineering. 1 edn, vol. 36, 012030, 1st International Conference on Mechanical Engineering Research 2011, ICMER 2011, Kuantan, Pahang, Malaysia, 5/12/11. https://doi.org/10.1088/1757-899X/36/1/012030
Eshkour RA, Mohd Ihsan AKA, Zulkifli R, Sulong AB, Azhari CH. The failure mode of natural silk epoxy triggered composite tubes. In IOP Conference Series: Materials Science and Engineering. 1 ed. Vol. 36. 2012. 012030 https://doi.org/10.1088/1757-899X/36/1/012030
Eshkour, R. A. ; Mohd Ihsan, Ahmad Kamal Ariffin ; Zulkifli, Rozli ; Sulong, Abu Bakar ; Azhari, Che Husna. / The failure mode of natural silk epoxy triggered composite tubes. IOP Conference Series: Materials Science and Engineering. Vol. 36 1. ed. 2012.
@inproceedings{1a4c56250ad441e69ac50e15a849f38d,
title = "The failure mode of natural silk epoxy triggered composite tubes",
abstract = "In this study the quasi static compression test over natural silk epoxy triggered composite tubes has been carried out, the natural silk epoxy composite tubes consist of 24 layer of woven natural silk as reinforcement and thermoset epoxy resin as matrix which both of them i e natural silk and epoxy have excellent mechanical properties More over the natural silk have better moisture resistance in comparison with other natural reinforcements, the length of tubes are 50, 80 and 120 mm The natural silk epoxy composite tubes are associated with an external trigger which includes 4 steel pieces welded on downside flat plate fixture The hand lay up fabrication method has been used to make the natural silk epoxy composite tubes Instron universal testing machine with 250 KN load capacity has been employed to accomplish this investigation The failure modes of natural silk epoxy triggered composite tubes has been investigated by representative photographs which has been taken by a high resolution camera(12 2 Mp) during the quasi static compression test, from the photographs is observed the failure modes is progressive local buckling",
author = "Eshkour, {R. A.} and {Mohd Ihsan}, {Ahmad Kamal Ariffin} and Rozli Zulkifli and Sulong, {Abu Bakar} and Azhari, {Che Husna}",
year = "2012",
doi = "10.1088/1757-899X/36/1/012030",
language = "English",
volume = "36",
booktitle = "IOP Conference Series: Materials Science and Engineering",
edition = "1",

}

TY - GEN

T1 - The failure mode of natural silk epoxy triggered composite tubes

AU - Eshkour, R. A.

AU - Mohd Ihsan, Ahmad Kamal Ariffin

AU - Zulkifli, Rozli

AU - Sulong, Abu Bakar

AU - Azhari, Che Husna

PY - 2012

Y1 - 2012

N2 - In this study the quasi static compression test over natural silk epoxy triggered composite tubes has been carried out, the natural silk epoxy composite tubes consist of 24 layer of woven natural silk as reinforcement and thermoset epoxy resin as matrix which both of them i e natural silk and epoxy have excellent mechanical properties More over the natural silk have better moisture resistance in comparison with other natural reinforcements, the length of tubes are 50, 80 and 120 mm The natural silk epoxy composite tubes are associated with an external trigger which includes 4 steel pieces welded on downside flat plate fixture The hand lay up fabrication method has been used to make the natural silk epoxy composite tubes Instron universal testing machine with 250 KN load capacity has been employed to accomplish this investigation The failure modes of natural silk epoxy triggered composite tubes has been investigated by representative photographs which has been taken by a high resolution camera(12 2 Mp) during the quasi static compression test, from the photographs is observed the failure modes is progressive local buckling

AB - In this study the quasi static compression test over natural silk epoxy triggered composite tubes has been carried out, the natural silk epoxy composite tubes consist of 24 layer of woven natural silk as reinforcement and thermoset epoxy resin as matrix which both of them i e natural silk and epoxy have excellent mechanical properties More over the natural silk have better moisture resistance in comparison with other natural reinforcements, the length of tubes are 50, 80 and 120 mm The natural silk epoxy composite tubes are associated with an external trigger which includes 4 steel pieces welded on downside flat plate fixture The hand lay up fabrication method has been used to make the natural silk epoxy composite tubes Instron universal testing machine with 250 KN load capacity has been employed to accomplish this investigation The failure modes of natural silk epoxy triggered composite tubes has been investigated by representative photographs which has been taken by a high resolution camera(12 2 Mp) during the quasi static compression test, from the photographs is observed the failure modes is progressive local buckling

UR - http://www.scopus.com/inward/record.url?scp=84874469726&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=84874469726&partnerID=8YFLogxK

U2 - 10.1088/1757-899X/36/1/012030

DO - 10.1088/1757-899X/36/1/012030

M3 - Conference contribution

VL - 36

BT - IOP Conference Series: Materials Science and Engineering

ER -