Stress distribution analysis on four types of stress corrosion cracking (SCC) specimen is presented in this paper. This work was performed using commercial finite element based software, ANSYS. Two types of mesh arrangements, fixed mesh with different mesh size and adaptive mesh, were employed in this work to study the effect of mesh size on stress distribution of SCC specimen. Four types of SCC specimen were studied in this work, i.e. C-ring specimen, tensile test specimen, pre-crack cantilever beam specimen and U-bend specimen. Simulation result shows that stress distribution on the SCC specimen much affected by mesh size and arrangement, especially for specimen with notch. By performing the stress analysis, less effort needed in order to determine the location of corrosion potential measurement on the SCC specimen. This will be very helpful for future work of SCC study.

Original languageEnglish
Title of host publicationKey Engineering Materials
Pages194-199
Number of pages6
Volume462-463
DOIs
Publication statusPublished - 2011
Event8th International Conference on Fracture and Strength of Solids 2010, FEOFS2010 - Kuala Lumpur
Duration: 7 Jun 20109 Jun 2010

Publication series

NameKey Engineering Materials
Volume462-463
ISSN (Print)10139826

Other

Other8th International Conference on Fracture and Strength of Solids 2010, FEOFS2010
CityKuala Lumpur
Period7/6/109/6/10

Fingerprint

Stress corrosion cracking
Stress concentration
Cantilever beams
Stress analysis
Corrosion
Cracks

Keywords

  • Adaptive mesh
  • ANSYS
  • Finite element analysis
  • Stress corrosion cracking

ASJC Scopus subject areas

  • Materials Science(all)
  • Mechanics of Materials
  • Mechanical Engineering

Cite this

Huzni, S., Ridha, M., & Mohd Ihsan, A. K. A. (2011). Stress distribution analysis on four types of stress corrosion cracking specimen. In Key Engineering Materials (Vol. 462-463, pp. 194-199). (Key Engineering Materials; Vol. 462-463). https://doi.org/10.4028/www.scientific.net/KEM.462-463.194

Stress distribution analysis on four types of stress corrosion cracking specimen. / Huzni, S.; Ridha, M.; Mohd Ihsan, Ahmad Kamal Ariffin.

Key Engineering Materials. Vol. 462-463 2011. p. 194-199 (Key Engineering Materials; Vol. 462-463).

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Huzni, S, Ridha, M & Mohd Ihsan, AKA 2011, Stress distribution analysis on four types of stress corrosion cracking specimen. in Key Engineering Materials. vol. 462-463, Key Engineering Materials, vol. 462-463, pp. 194-199, 8th International Conference on Fracture and Strength of Solids 2010, FEOFS2010, Kuala Lumpur, 7/6/10. https://doi.org/10.4028/www.scientific.net/KEM.462-463.194
Huzni S, Ridha M, Mohd Ihsan AKA. Stress distribution analysis on four types of stress corrosion cracking specimen. In Key Engineering Materials. Vol. 462-463. 2011. p. 194-199. (Key Engineering Materials). https://doi.org/10.4028/www.scientific.net/KEM.462-463.194
Huzni, S. ; Ridha, M. ; Mohd Ihsan, Ahmad Kamal Ariffin. / Stress distribution analysis on four types of stress corrosion cracking specimen. Key Engineering Materials. Vol. 462-463 2011. pp. 194-199 (Key Engineering Materials).
@inproceedings{2843af94976d4f7fb8998c68edf50317,
title = "Stress distribution analysis on four types of stress corrosion cracking specimen",
abstract = "Stress distribution analysis on four types of stress corrosion cracking (SCC) specimen is presented in this paper. This work was performed using commercial finite element based software, ANSYS. Two types of mesh arrangements, fixed mesh with different mesh size and adaptive mesh, were employed in this work to study the effect of mesh size on stress distribution of SCC specimen. Four types of SCC specimen were studied in this work, i.e. C-ring specimen, tensile test specimen, pre-crack cantilever beam specimen and U-bend specimen. Simulation result shows that stress distribution on the SCC specimen much affected by mesh size and arrangement, especially for specimen with notch. By performing the stress analysis, less effort needed in order to determine the location of corrosion potential measurement on the SCC specimen. This will be very helpful for future work of SCC study.",
keywords = "Adaptive mesh, ANSYS, Finite element analysis, Stress corrosion cracking",
author = "S. Huzni and M. Ridha and {Mohd Ihsan}, {Ahmad Kamal Ariffin}",
year = "2011",
doi = "10.4028/www.scientific.net/KEM.462-463.194",
language = "English",
isbn = "9780878492107",
volume = "462-463",
series = "Key Engineering Materials",
pages = "194--199",
booktitle = "Key Engineering Materials",

}

TY - GEN

T1 - Stress distribution analysis on four types of stress corrosion cracking specimen

AU - Huzni, S.

AU - Ridha, M.

AU - Mohd Ihsan, Ahmad Kamal Ariffin

PY - 2011

Y1 - 2011

N2 - Stress distribution analysis on four types of stress corrosion cracking (SCC) specimen is presented in this paper. This work was performed using commercial finite element based software, ANSYS. Two types of mesh arrangements, fixed mesh with different mesh size and adaptive mesh, were employed in this work to study the effect of mesh size on stress distribution of SCC specimen. Four types of SCC specimen were studied in this work, i.e. C-ring specimen, tensile test specimen, pre-crack cantilever beam specimen and U-bend specimen. Simulation result shows that stress distribution on the SCC specimen much affected by mesh size and arrangement, especially for specimen with notch. By performing the stress analysis, less effort needed in order to determine the location of corrosion potential measurement on the SCC specimen. This will be very helpful for future work of SCC study.

AB - Stress distribution analysis on four types of stress corrosion cracking (SCC) specimen is presented in this paper. This work was performed using commercial finite element based software, ANSYS. Two types of mesh arrangements, fixed mesh with different mesh size and adaptive mesh, were employed in this work to study the effect of mesh size on stress distribution of SCC specimen. Four types of SCC specimen were studied in this work, i.e. C-ring specimen, tensile test specimen, pre-crack cantilever beam specimen and U-bend specimen. Simulation result shows that stress distribution on the SCC specimen much affected by mesh size and arrangement, especially for specimen with notch. By performing the stress analysis, less effort needed in order to determine the location of corrosion potential measurement on the SCC specimen. This will be very helpful for future work of SCC study.

KW - Adaptive mesh

KW - ANSYS

KW - Finite element analysis

KW - Stress corrosion cracking

UR - http://www.scopus.com/inward/record.url?scp=79551481523&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=79551481523&partnerID=8YFLogxK

U2 - 10.4028/www.scientific.net/KEM.462-463.194

DO - 10.4028/www.scientific.net/KEM.462-463.194

M3 - Conference contribution

SN - 9780878492107

VL - 462-463

T3 - Key Engineering Materials

SP - 194

EP - 199

BT - Key Engineering Materials

ER -