Abstract

Ethyl violet (EV) and methyl orange (MO) are commercial dyes used in a large number of industries. Due to their complex chemical structures and synthetic nature, these dyes are highly stable to light and oxidation, making them non-biodegradable, highly toxic, carcinogenic and mutagenic in nature. Among all techniques, adsorption continues to attract considerable attention due to its simplistic approach and numerous benefits such as greater efficiency, capacity to remove dyes on a large scale, ease of recovery, and recyclability of adsorbents. A palm-based polyurethane (PU) membrane has been synthesised into adsorbent and its ability to adsorb the dye molecules was investigated. The PU membrane was produced via condensation polymerisation between palm-based monoester (PKOp) and 4,4-methylene diphenyl diisocyanate (MDI) with acetone as the solvent. The FTIR spectrum has confirmed the formation of urethane linkage (HN-(C)O) through the presence of N-H, C-NH, C-O-C and C=O urethane peaks which were observed at 3293 cm -1 , 1602cm -1 , 1221 cm -1 dan 1716 cm -1 , respectively. Tensile testing has demonstrated that as the thickness of membrane is increased, the elasticity also increased proportionally with increasing tensile strain ranging from 6.7 MPa to 7.42 MPa. Various adsorption parameters such as initial concentration of dyes, effect of pH, effect of adsorbent dosage and contact time were studied and optimised. The adsorption study revealed that approximately 99% of EV and 25% of MO was adsorbed by the PU membrane within a short duration of 30 minutes. The parameters were determined from Langmuir, Freundlich and Temkin adsorption isotherm models. The isotherm studies specified that the adsorption of PU membrane towards EV and MO dyes is well fitted to the Langmuir model with the value of the maximum adsorption capacities for monolayer adsorption at 9.461 mg/g for EV and 4.340 mg/g for MO.

Original languageMalay
Pages (from-to)1040-1047
Number of pages8
JournalMalaysian Journal of Analytical Sciences
Volume22
Issue number6
DOIs
Publication statusPublished - 1 Dec 2018

Fingerprint

Polyurethanes
Adsorbents
Coloring Agents
Membranes
Adsorption
Urethane
pH effects
Tensile strain
Poisons
Tensile testing
Polycondensation
Acetone
Adsorption isotherms
Isotherms
methyl orange
ethyl violet
Elasticity
Monolayers
Recovery
Oxidation

ASJC Scopus subject areas

  • Analytical Chemistry

Cite this

Membran poliuretana sebagai penjerap untuk pewarna metil oren dan etil ungu lembayung. / Badri, Khairiah; Ismail, Fatem Hamimie; Shakir, Amira Shakim Abdul; Mohamad, Sharifah; Hamuzan, Hawa Aqilah; Hassan, Nur Syakilla.

In: Malaysian Journal of Analytical Sciences, Vol. 22, No. 6, 01.12.2018, p. 1040-1047.

Research output: Contribution to journalArticle

Badri, Khairiah ; Ismail, Fatem Hamimie ; Shakir, Amira Shakim Abdul ; Mohamad, Sharifah ; Hamuzan, Hawa Aqilah ; Hassan, Nur Syakilla. / Membran poliuretana sebagai penjerap untuk pewarna metil oren dan etil ungu lembayung. In: Malaysian Journal of Analytical Sciences. 2018 ; Vol. 22, No. 6. pp. 1040-1047.
@article{e2936de327884408afdf4e9fe819c964,
title = "Membran poliuretana sebagai penjerap untuk pewarna metil oren dan etil ungu lembayung",
abstract = "Ethyl violet (EV) and methyl orange (MO) are commercial dyes used in a large number of industries. Due to their complex chemical structures and synthetic nature, these dyes are highly stable to light and oxidation, making them non-biodegradable, highly toxic, carcinogenic and mutagenic in nature. Among all techniques, adsorption continues to attract considerable attention due to its simplistic approach and numerous benefits such as greater efficiency, capacity to remove dyes on a large scale, ease of recovery, and recyclability of adsorbents. A palm-based polyurethane (PU) membrane has been synthesised into adsorbent and its ability to adsorb the dye molecules was investigated. The PU membrane was produced via condensation polymerisation between palm-based monoester (PKOp) and 4,4-methylene diphenyl diisocyanate (MDI) with acetone as the solvent. The FTIR spectrum has confirmed the formation of urethane linkage (HN-(C)O) through the presence of N-H, C-NH, C-O-C and C=O urethane peaks which were observed at 3293 cm -1 , 1602cm -1 , 1221 cm -1 dan 1716 cm -1 , respectively. Tensile testing has demonstrated that as the thickness of membrane is increased, the elasticity also increased proportionally with increasing tensile strain ranging from 6.7 MPa to 7.42 MPa. Various adsorption parameters such as initial concentration of dyes, effect of pH, effect of adsorbent dosage and contact time were studied and optimised. The adsorption study revealed that approximately 99{\%} of EV and 25{\%} of MO was adsorbed by the PU membrane within a short duration of 30 minutes. The parameters were determined from Langmuir, Freundlich and Temkin adsorption isotherm models. The isotherm studies specified that the adsorption of PU membrane towards EV and MO dyes is well fitted to the Langmuir model with the value of the maximum adsorption capacities for monolayer adsorption at 9.461 mg/g for EV and 4.340 mg/g for MO.",
keywords = "Adsorption, Adsorption isotherm, Ethyl violet, Methyl orange, Polyurethane membrane",
author = "Khairiah Badri and Ismail, {Fatem Hamimie} and Shakir, {Amira Shakim Abdul} and Sharifah Mohamad and Hamuzan, {Hawa Aqilah} and Hassan, {Nur Syakilla}",
year = "2018",
month = "12",
day = "1",
doi = "10.17576/mjas-2018-2206-14",
language = "Malay",
volume = "22",
pages = "1040--1047",
journal = "Malaysian Journal of Analytical Sciences",
issn = "1394-2506",
publisher = "Faculty of Science and Technology, Universiti Kebangsaan Malaysia",
number = "6",

}

TY - JOUR

T1 - Membran poliuretana sebagai penjerap untuk pewarna metil oren dan etil ungu lembayung

AU - Badri, Khairiah

AU - Ismail, Fatem Hamimie

AU - Shakir, Amira Shakim Abdul

AU - Mohamad, Sharifah

AU - Hamuzan, Hawa Aqilah

AU - Hassan, Nur Syakilla

PY - 2018/12/1

Y1 - 2018/12/1

N2 - Ethyl violet (EV) and methyl orange (MO) are commercial dyes used in a large number of industries. Due to their complex chemical structures and synthetic nature, these dyes are highly stable to light and oxidation, making them non-biodegradable, highly toxic, carcinogenic and mutagenic in nature. Among all techniques, adsorption continues to attract considerable attention due to its simplistic approach and numerous benefits such as greater efficiency, capacity to remove dyes on a large scale, ease of recovery, and recyclability of adsorbents. A palm-based polyurethane (PU) membrane has been synthesised into adsorbent and its ability to adsorb the dye molecules was investigated. The PU membrane was produced via condensation polymerisation between palm-based monoester (PKOp) and 4,4-methylene diphenyl diisocyanate (MDI) with acetone as the solvent. The FTIR spectrum has confirmed the formation of urethane linkage (HN-(C)O) through the presence of N-H, C-NH, C-O-C and C=O urethane peaks which were observed at 3293 cm -1 , 1602cm -1 , 1221 cm -1 dan 1716 cm -1 , respectively. Tensile testing has demonstrated that as the thickness of membrane is increased, the elasticity also increased proportionally with increasing tensile strain ranging from 6.7 MPa to 7.42 MPa. Various adsorption parameters such as initial concentration of dyes, effect of pH, effect of adsorbent dosage and contact time were studied and optimised. The adsorption study revealed that approximately 99% of EV and 25% of MO was adsorbed by the PU membrane within a short duration of 30 minutes. The parameters were determined from Langmuir, Freundlich and Temkin adsorption isotherm models. The isotherm studies specified that the adsorption of PU membrane towards EV and MO dyes is well fitted to the Langmuir model with the value of the maximum adsorption capacities for monolayer adsorption at 9.461 mg/g for EV and 4.340 mg/g for MO.

AB - Ethyl violet (EV) and methyl orange (MO) are commercial dyes used in a large number of industries. Due to their complex chemical structures and synthetic nature, these dyes are highly stable to light and oxidation, making them non-biodegradable, highly toxic, carcinogenic and mutagenic in nature. Among all techniques, adsorption continues to attract considerable attention due to its simplistic approach and numerous benefits such as greater efficiency, capacity to remove dyes on a large scale, ease of recovery, and recyclability of adsorbents. A palm-based polyurethane (PU) membrane has been synthesised into adsorbent and its ability to adsorb the dye molecules was investigated. The PU membrane was produced via condensation polymerisation between palm-based monoester (PKOp) and 4,4-methylene diphenyl diisocyanate (MDI) with acetone as the solvent. The FTIR spectrum has confirmed the formation of urethane linkage (HN-(C)O) through the presence of N-H, C-NH, C-O-C and C=O urethane peaks which were observed at 3293 cm -1 , 1602cm -1 , 1221 cm -1 dan 1716 cm -1 , respectively. Tensile testing has demonstrated that as the thickness of membrane is increased, the elasticity also increased proportionally with increasing tensile strain ranging from 6.7 MPa to 7.42 MPa. Various adsorption parameters such as initial concentration of dyes, effect of pH, effect of adsorbent dosage and contact time were studied and optimised. The adsorption study revealed that approximately 99% of EV and 25% of MO was adsorbed by the PU membrane within a short duration of 30 minutes. The parameters were determined from Langmuir, Freundlich and Temkin adsorption isotherm models. The isotherm studies specified that the adsorption of PU membrane towards EV and MO dyes is well fitted to the Langmuir model with the value of the maximum adsorption capacities for monolayer adsorption at 9.461 mg/g for EV and 4.340 mg/g for MO.

KW - Adsorption

KW - Adsorption isotherm

KW - Ethyl violet

KW - Methyl orange

KW - Polyurethane membrane

UR - http://www.scopus.com/inward/record.url?scp=85061233366&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=85061233366&partnerID=8YFLogxK

U2 - 10.17576/mjas-2018-2206-14

DO - 10.17576/mjas-2018-2206-14

M3 - Article

AN - SCOPUS:85061233366

VL - 22

SP - 1040

EP - 1047

JO - Malaysian Journal of Analytical Sciences

JF - Malaysian Journal of Analytical Sciences

SN - 1394-2506

IS - 6

ER -