Inhibition of galvanic corrosion was carried out using 4-amino-5-phenyl-4H- 1, 2, 4-trizole-3-thiol (APTT) as corrosion inhibitor. The couple metals were aluminium alloy (Al2024) and mild steel. The galvanic potential and the galvanic current were measured in absence and presence of 0.4 mM of APTT. FT-IR was used to characterise the adsorbed inhibitor film technique. The result showed that the galvanic current was reduced from 286 to 8.9 μA cm-2 with addition of APTT. FTIR result confirmed the adsorption of APTT on mild steel surface.

Original languageEnglish
Pages (from-to)226-231
Number of pages6
JournalInternational Journal of Surface Science and Engineering
Volume5
Issue number2-3
DOIs
Publication statusPublished - Jul 2011

Fingerprint

Sulfhydryl Compounds
thiols
inhibitors
Carbon steel
corrosion
steels
Corrosion
Alloy steel
Corrosion inhibitors
aluminum alloys
Aluminum alloys
Metals
Adsorption
adsorption
metals

Keywords

  • Corrosion inhibitor
  • Fourier transform infrared
  • FTIR
  • Galvanic corrosion
  • Zero resistance ammeter
  • ZRA

ASJC Scopus subject areas

  • Mechanical Engineering
  • Surfaces, Coatings and Films
  • Surfaces and Interfaces

Cite this

Inhibition of galvanic corrosion by 4-amino-5-phenyl-4H-1, 2, 4-trizole-3-thiol. / Musa, Ahmed Y.; Kadhum, Abdul Amir H.; Takriff, Mohd Sobri; Mohamad, Abu Bakar.

In: International Journal of Surface Science and Engineering, Vol. 5, No. 2-3, 07.2011, p. 226-231.

Research output: Contribution to journalArticle

Musa, Ahmed Y. ; Kadhum, Abdul Amir H. ; Takriff, Mohd Sobri ; Mohamad, Abu Bakar. / Inhibition of galvanic corrosion by 4-amino-5-phenyl-4H-1, 2, 4-trizole-3-thiol. In: International Journal of Surface Science and Engineering. 2011 ; Vol. 5, No. 2-3. pp. 226-231.
@article{91cd65c2ee564b2d9db3a01f33e66999,
title = "Inhibition of galvanic corrosion by 4-amino-5-phenyl-4H-1, 2, 4-trizole-3-thiol",
abstract = "Inhibition of galvanic corrosion was carried out using 4-amino-5-phenyl-4H- 1, 2, 4-trizole-3-thiol (APTT) as corrosion inhibitor. The couple metals were aluminium alloy (Al2024) and mild steel. The galvanic potential and the galvanic current were measured in absence and presence of 0.4 mM of APTT. FT-IR was used to characterise the adsorbed inhibitor film technique. The result showed that the galvanic current was reduced from 286 to 8.9 μA cm-2 with addition of APTT. FTIR result confirmed the adsorption of APTT on mild steel surface.",
keywords = "Corrosion inhibitor, Fourier transform infrared, FTIR, Galvanic corrosion, Zero resistance ammeter, ZRA",
author = "Musa, {Ahmed Y.} and Kadhum, {Abdul Amir H.} and Takriff, {Mohd Sobri} and Mohamad, {Abu Bakar}",
year = "2011",
month = "7",
doi = "10.1504/IJSURFSE.2011.041405",
language = "English",
volume = "5",
pages = "226--231",
journal = "International Journal of Surface Science and Engineering",
issn = "1749-785X",
publisher = "Inderscience Enterprises Ltd",
number = "2-3",

}

TY - JOUR

T1 - Inhibition of galvanic corrosion by 4-amino-5-phenyl-4H-1, 2, 4-trizole-3-thiol

AU - Musa, Ahmed Y.

AU - Kadhum, Abdul Amir H.

AU - Takriff, Mohd Sobri

AU - Mohamad, Abu Bakar

PY - 2011/7

Y1 - 2011/7

N2 - Inhibition of galvanic corrosion was carried out using 4-amino-5-phenyl-4H- 1, 2, 4-trizole-3-thiol (APTT) as corrosion inhibitor. The couple metals were aluminium alloy (Al2024) and mild steel. The galvanic potential and the galvanic current were measured in absence and presence of 0.4 mM of APTT. FT-IR was used to characterise the adsorbed inhibitor film technique. The result showed that the galvanic current was reduced from 286 to 8.9 μA cm-2 with addition of APTT. FTIR result confirmed the adsorption of APTT on mild steel surface.

AB - Inhibition of galvanic corrosion was carried out using 4-amino-5-phenyl-4H- 1, 2, 4-trizole-3-thiol (APTT) as corrosion inhibitor. The couple metals were aluminium alloy (Al2024) and mild steel. The galvanic potential and the galvanic current were measured in absence and presence of 0.4 mM of APTT. FT-IR was used to characterise the adsorbed inhibitor film technique. The result showed that the galvanic current was reduced from 286 to 8.9 μA cm-2 with addition of APTT. FTIR result confirmed the adsorption of APTT on mild steel surface.

KW - Corrosion inhibitor

KW - Fourier transform infrared

KW - FTIR

KW - Galvanic corrosion

KW - Zero resistance ammeter

KW - ZRA

UR - http://www.scopus.com/inward/record.url?scp=79960823488&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=79960823488&partnerID=8YFLogxK

U2 - 10.1504/IJSURFSE.2011.041405

DO - 10.1504/IJSURFSE.2011.041405

M3 - Article

AN - SCOPUS:79960823488

VL - 5

SP - 226

EP - 231

JO - International Journal of Surface Science and Engineering

JF - International Journal of Surface Science and Engineering

SN - 1749-785X

IS - 2-3

ER -