Effect of the deposition time on LSCF-SDC carbonate thin film formation by the electrophoretic deposition method

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Abstract

La0.6Sr0.4Co0.2Fe0.8O3-δ-samarium-doped ceria (SDC) carbonate thin films are produced on SDC carbonate substrates by the electrophoretic deposition (EPD) method. EPD is performed by fixing the voltage and suspension pH while varying the deposition time to obtain a >20 μm-thick layer. The deposition time of 30 min yields more particle deposits than 10, 15, 20, and 25 min. Thin films with an average thickness of 22.9050 μm are obtained from the EPD technique when the voltage is 20 V and the suspension pH is 5.

Original languageEnglish
Title of host publicationAdvanced Materials Research
Pages1813-1818
Number of pages6
Volume616-618
DOIs
Publication statusPublished - 2013
Event2nd International Conference on Energy, Environment and Sustainable Development, EESD 2012 - Jilin
Duration: 12 Oct 201214 Oct 2012

Publication series

NameAdvanced Materials Research
Volume616-618
ISSN (Print)10226680

Other

Other2nd International Conference on Energy, Environment and Sustainable Development, EESD 2012
CityJilin
Period12/10/1214/10/12

Fingerprint

Samarium
Cerium compounds
Carbonates
Thin films
Electric potential
Deposits
Substrates

Keywords

  • Deposition time
  • Electrophoretic deposition (EPD)
  • La0.6Sr0.4Co0.2Fe0.8O3-δ-samarium doped-ceria carbonates (LSCF-SDCC)

ASJC Scopus subject areas

  • Engineering(all)

Cite this

Effect of the deposition time on LSCF-SDC carbonate thin film formation by the electrophoretic deposition method. / Baharuddin, Nurul Akidah; Muchtar, Andanastuti; Sulong, Abu Bakar; Abdullah, Huda.

Advanced Materials Research. Vol. 616-618 2013. p. 1813-1818 (Advanced Materials Research; Vol. 616-618).

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Baharuddin, NA, Muchtar, A, Sulong, AB & Abdullah, H 2013, Effect of the deposition time on LSCF-SDC carbonate thin film formation by the electrophoretic deposition method. in Advanced Materials Research. vol. 616-618, Advanced Materials Research, vol. 616-618, pp. 1813-1818, 2nd International Conference on Energy, Environment and Sustainable Development, EESD 2012, Jilin, 12/10/12. https://doi.org/10.4028/www.scientific.net/AMR.616-618.1813
Baharuddin, Nurul Akidah ; Muchtar, Andanastuti ; Sulong, Abu Bakar ; Abdullah, Huda. / Effect of the deposition time on LSCF-SDC carbonate thin film formation by the electrophoretic deposition method. Advanced Materials Research. Vol. 616-618 2013. pp. 1813-1818 (Advanced Materials Research).
@inproceedings{6b7009052dcd467eb46015d7acd793d7,
title = "Effect of the deposition time on LSCF-SDC carbonate thin film formation by the electrophoretic deposition method",
abstract = "La0.6Sr0.4Co0.2Fe0.8O3-δ-samarium-doped ceria (SDC) carbonate thin films are produced on SDC carbonate substrates by the electrophoretic deposition (EPD) method. EPD is performed by fixing the voltage and suspension pH while varying the deposition time to obtain a >20 μm-thick layer. The deposition time of 30 min yields more particle deposits than 10, 15, 20, and 25 min. Thin films with an average thickness of 22.9050 μm are obtained from the EPD technique when the voltage is 20 V and the suspension pH is 5.",
keywords = "Deposition time, Electrophoretic deposition (EPD), La0.6Sr0.4Co0.2Fe0.8O3-δ-samarium doped-ceria carbonates (LSCF-SDCC)",
author = "Baharuddin, {Nurul Akidah} and Andanastuti Muchtar and Sulong, {Abu Bakar} and Huda Abdullah",
year = "2013",
doi = "10.4028/www.scientific.net/AMR.616-618.1813",
language = "English",
isbn = "9783037855522",
volume = "616-618",
series = "Advanced Materials Research",
pages = "1813--1818",
booktitle = "Advanced Materials Research",

}

TY - GEN

T1 - Effect of the deposition time on LSCF-SDC carbonate thin film formation by the electrophoretic deposition method

AU - Baharuddin, Nurul Akidah

AU - Muchtar, Andanastuti

AU - Sulong, Abu Bakar

AU - Abdullah, Huda

PY - 2013

Y1 - 2013

N2 - La0.6Sr0.4Co0.2Fe0.8O3-δ-samarium-doped ceria (SDC) carbonate thin films are produced on SDC carbonate substrates by the electrophoretic deposition (EPD) method. EPD is performed by fixing the voltage and suspension pH while varying the deposition time to obtain a >20 μm-thick layer. The deposition time of 30 min yields more particle deposits than 10, 15, 20, and 25 min. Thin films with an average thickness of 22.9050 μm are obtained from the EPD technique when the voltage is 20 V and the suspension pH is 5.

AB - La0.6Sr0.4Co0.2Fe0.8O3-δ-samarium-doped ceria (SDC) carbonate thin films are produced on SDC carbonate substrates by the electrophoretic deposition (EPD) method. EPD is performed by fixing the voltage and suspension pH while varying the deposition time to obtain a >20 μm-thick layer. The deposition time of 30 min yields more particle deposits than 10, 15, 20, and 25 min. Thin films with an average thickness of 22.9050 μm are obtained from the EPD technique when the voltage is 20 V and the suspension pH is 5.

KW - Deposition time

KW - Electrophoretic deposition (EPD)

KW - La0.6Sr0.4Co0.2Fe0.8O3-δ-samarium doped-ceria carbonates (LSCF-SDCC)

UR - http://www.scopus.com/inward/record.url?scp=84871861489&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=84871861489&partnerID=8YFLogxK

U2 - 10.4028/www.scientific.net/AMR.616-618.1813

DO - 10.4028/www.scientific.net/AMR.616-618.1813

M3 - Conference contribution

SN - 9783037855522

VL - 616-618

T3 - Advanced Materials Research

SP - 1813

EP - 1818

BT - Advanced Materials Research

ER -