Effect of nanoindentation loading rate on gold ball bond

Muhammad Nubli Zulkifli, Azman Jalar @ Jalil, Shahrum Abdullah

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Abstract

Nanoindentation tests with loading rates of 0.05 mN/s, 0.1 mN/s, 0.5 mN/s, and 1.0 mN/s were conducted on the Au ball bond. The effect of different loading on the Au ball bond were analysed based on qualitative and quantitative results. The displacement burst was more pronounced with the increment of loading rates. The increase of hardness value and the decrease of the reduced modulus value when the loading rate was increased are due to the effect of creep. It was found that the loading rate of 0.5 mN/s is the appropriate and stable value for the nanoindentation test on the Au ball bond.

Original languageEnglish
Title of host publicationMaterials Science Forum
Pages151-155
Number of pages5
Volume756
DOIs
Publication statusPublished - 2013
Event3rd ISESCO International Workshop and Conference on Nanotechnology 2012, IWCN 2012 - Selangor
Duration: 5 Dec 20127 Dec 2012

Publication series

NameMaterials Science Forum
Volume756
ISSN (Print)02555476

Other

Other3rd ISESCO International Workshop and Conference on Nanotechnology 2012, IWCN 2012
CitySelangor
Period5/12/127/12/12

Fingerprint

loading rate
Nanoindentation
nanoindentation
Gold
balls
gold
Creep
Hardness
bursts
hardness

Keywords

  • Gold ball bond
  • Loading rate
  • Nanoindentation
  • Wire bonding

ASJC Scopus subject areas

  • Materials Science(all)
  • Condensed Matter Physics
  • Mechanical Engineering
  • Mechanics of Materials

Cite this

Zulkifli, M. N., Jalar @ Jalil, A., & Abdullah, S. (2013). Effect of nanoindentation loading rate on gold ball bond. In Materials Science Forum (Vol. 756, pp. 151-155). (Materials Science Forum; Vol. 756). https://doi.org/10.4028/www.scientific.net/MSF.756.151

Effect of nanoindentation loading rate on gold ball bond. / Zulkifli, Muhammad Nubli; Jalar @ Jalil, Azman; Abdullah, Shahrum.

Materials Science Forum. Vol. 756 2013. p. 151-155 (Materials Science Forum; Vol. 756).

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Zulkifli, MN, Jalar @ Jalil, A & Abdullah, S 2013, Effect of nanoindentation loading rate on gold ball bond. in Materials Science Forum. vol. 756, Materials Science Forum, vol. 756, pp. 151-155, 3rd ISESCO International Workshop and Conference on Nanotechnology 2012, IWCN 2012, Selangor, 5/12/12. https://doi.org/10.4028/www.scientific.net/MSF.756.151
Zulkifli MN, Jalar @ Jalil A, Abdullah S. Effect of nanoindentation loading rate on gold ball bond. In Materials Science Forum. Vol. 756. 2013. p. 151-155. (Materials Science Forum). https://doi.org/10.4028/www.scientific.net/MSF.756.151
Zulkifli, Muhammad Nubli ; Jalar @ Jalil, Azman ; Abdullah, Shahrum. / Effect of nanoindentation loading rate on gold ball bond. Materials Science Forum. Vol. 756 2013. pp. 151-155 (Materials Science Forum).
@inproceedings{70cb1aa2a0394eb79a1d548f4cdfc207,
title = "Effect of nanoindentation loading rate on gold ball bond",
abstract = "Nanoindentation tests with loading rates of 0.05 mN/s, 0.1 mN/s, 0.5 mN/s, and 1.0 mN/s were conducted on the Au ball bond. The effect of different loading on the Au ball bond were analysed based on qualitative and quantitative results. The displacement burst was more pronounced with the increment of loading rates. The increase of hardness value and the decrease of the reduced modulus value when the loading rate was increased are due to the effect of creep. It was found that the loading rate of 0.5 mN/s is the appropriate and stable value for the nanoindentation test on the Au ball bond.",
keywords = "Gold ball bond, Loading rate, Nanoindentation, Wire bonding",
author = "Zulkifli, {Muhammad Nubli} and {Jalar @ Jalil}, Azman and Shahrum Abdullah",
year = "2013",
doi = "10.4028/www.scientific.net/MSF.756.151",
language = "English",
isbn = "9783037856956",
volume = "756",
series = "Materials Science Forum",
pages = "151--155",
booktitle = "Materials Science Forum",

}

TY - GEN

T1 - Effect of nanoindentation loading rate on gold ball bond

AU - Zulkifli, Muhammad Nubli

AU - Jalar @ Jalil, Azman

AU - Abdullah, Shahrum

PY - 2013

Y1 - 2013

N2 - Nanoindentation tests with loading rates of 0.05 mN/s, 0.1 mN/s, 0.5 mN/s, and 1.0 mN/s were conducted on the Au ball bond. The effect of different loading on the Au ball bond were analysed based on qualitative and quantitative results. The displacement burst was more pronounced with the increment of loading rates. The increase of hardness value and the decrease of the reduced modulus value when the loading rate was increased are due to the effect of creep. It was found that the loading rate of 0.5 mN/s is the appropriate and stable value for the nanoindentation test on the Au ball bond.

AB - Nanoindentation tests with loading rates of 0.05 mN/s, 0.1 mN/s, 0.5 mN/s, and 1.0 mN/s were conducted on the Au ball bond. The effect of different loading on the Au ball bond were analysed based on qualitative and quantitative results. The displacement burst was more pronounced with the increment of loading rates. The increase of hardness value and the decrease of the reduced modulus value when the loading rate was increased are due to the effect of creep. It was found that the loading rate of 0.5 mN/s is the appropriate and stable value for the nanoindentation test on the Au ball bond.

KW - Gold ball bond

KW - Loading rate

KW - Nanoindentation

KW - Wire bonding

UR - http://www.scopus.com/inward/record.url?scp=84878479380&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=84878479380&partnerID=8YFLogxK

U2 - 10.4028/www.scientific.net/MSF.756.151

DO - 10.4028/www.scientific.net/MSF.756.151

M3 - Conference contribution

AN - SCOPUS:84878479380

SN - 9783037856956

VL - 756

T3 - Materials Science Forum

SP - 151

EP - 155

BT - Materials Science Forum

ER -