Abstract

Stone Mastic Asphalt (SMA) mixtures are designed to have a high coarse aggregate content and stone-on-stone contact, which results in more stress on the coarse aggregates during compaction and traffic loading. As a result, aggregates tend to break down more in SMA mixtures than in conventional dense graded mixtures. Aggregate degradation during compaction and traffic loading may cause changes in the original gradation and thus may also affect the volumetric parameters of SMA mixtures. Therefore, this study was conducted to determine the degree of aggregate degradation in SMA mixtures due to the compaction process. Aggregates of two Nominal Maximum Aggregates Sizes (NMAS), designated as SMA14 and SMA20, were compacted using 50 blows of the Marshall Hammer and 100 gyrations of the Superpave Gyratory Compactor (SGC). The verified samples were then prepared and extracted using the Centrifuge Method. The relationship between aggregate degradation and influencing factors, such as compaction effort and volumetric properties were investigated. Aggregate degradation by the Marshall Hammer was found to be significantly higher than degradation by the SGC. Voids in the mineral aggregate (VMA) of either compaction method decrease or are almost the same when aggregate degradation is not significant. SGC method can be selected to represent the field roller that results in a similar trend of aggregate degradation.

Original languageEnglish
Pages (from-to)111-114
Number of pages4
JournalJurnal Teknologi (Sciences and Engineering)
Volume65
Issue number3
DOIs
Publication statusPublished - 2013

Fingerprint

Mastic asphalt
Asphalt mixtures
Degradation
Superpave
Compaction
Hammers
Centrifuges

Keywords

  • Aggregate
  • Compaction
  • Degradation
  • Gyratory
  • Marshall

ASJC Scopus subject areas

  • Engineering(all)

Cite this

Hainin, M. R., Akhir, N. M., Jaya, R. P., Md Yusoff, N. I., Yaacob, H., Ismail, C. R., & Hassan, N. A. (2013). Aggregate degradation characteristics of stone mastic asphalt mixtures. Jurnal Teknologi (Sciences and Engineering), 65(3), 111-114. https://doi.org/10.11113/jt.v65.2155

Aggregate degradation characteristics of stone mastic asphalt mixtures. / Hainin, Mohd Rosli; Akhir, Norliza Mohd; Jaya, Ramadhansyah Putra; Md Yusoff, Nur Izzi; Yaacob, Haryati; Ismail, Che Ros; Hassan, Norhidayah Abdul.

In: Jurnal Teknologi (Sciences and Engineering), Vol. 65, No. 3, 2013, p. 111-114.

Research output: Contribution to journalArticle

Hainin, Mohd Rosli ; Akhir, Norliza Mohd ; Jaya, Ramadhansyah Putra ; Md Yusoff, Nur Izzi ; Yaacob, Haryati ; Ismail, Che Ros ; Hassan, Norhidayah Abdul. / Aggregate degradation characteristics of stone mastic asphalt mixtures. In: Jurnal Teknologi (Sciences and Engineering). 2013 ; Vol. 65, No. 3. pp. 111-114.
@article{9f3bdc0118e34f218ada67e7ca6622af,
title = "Aggregate degradation characteristics of stone mastic asphalt mixtures",
abstract = "Stone Mastic Asphalt (SMA) mixtures are designed to have a high coarse aggregate content and stone-on-stone contact, which results in more stress on the coarse aggregates during compaction and traffic loading. As a result, aggregates tend to break down more in SMA mixtures than in conventional dense graded mixtures. Aggregate degradation during compaction and traffic loading may cause changes in the original gradation and thus may also affect the volumetric parameters of SMA mixtures. Therefore, this study was conducted to determine the degree of aggregate degradation in SMA mixtures due to the compaction process. Aggregates of two Nominal Maximum Aggregates Sizes (NMAS), designated as SMA14 and SMA20, were compacted using 50 blows of the Marshall Hammer and 100 gyrations of the Superpave Gyratory Compactor (SGC). The verified samples were then prepared and extracted using the Centrifuge Method. The relationship between aggregate degradation and influencing factors, such as compaction effort and volumetric properties were investigated. Aggregate degradation by the Marshall Hammer was found to be significantly higher than degradation by the SGC. Voids in the mineral aggregate (VMA) of either compaction method decrease or are almost the same when aggregate degradation is not significant. SGC method can be selected to represent the field roller that results in a similar trend of aggregate degradation.",
keywords = "Aggregate, Compaction, Degradation, Gyratory, Marshall",
author = "Hainin, {Mohd Rosli} and Akhir, {Norliza Mohd} and Jaya, {Ramadhansyah Putra} and {Md Yusoff}, {Nur Izzi} and Haryati Yaacob and Ismail, {Che Ros} and Hassan, {Norhidayah Abdul}",
year = "2013",
doi = "10.11113/jt.v65.2155",
language = "English",
volume = "65",
pages = "111--114",
journal = "Jurnal Teknologi",
issn = "0127-9696",
publisher = "Penerbit Universiti Teknologi Malaysia",
number = "3",

}

TY - JOUR

T1 - Aggregate degradation characteristics of stone mastic asphalt mixtures

AU - Hainin, Mohd Rosli

AU - Akhir, Norliza Mohd

AU - Jaya, Ramadhansyah Putra

AU - Md Yusoff, Nur Izzi

AU - Yaacob, Haryati

AU - Ismail, Che Ros

AU - Hassan, Norhidayah Abdul

PY - 2013

Y1 - 2013

N2 - Stone Mastic Asphalt (SMA) mixtures are designed to have a high coarse aggregate content and stone-on-stone contact, which results in more stress on the coarse aggregates during compaction and traffic loading. As a result, aggregates tend to break down more in SMA mixtures than in conventional dense graded mixtures. Aggregate degradation during compaction and traffic loading may cause changes in the original gradation and thus may also affect the volumetric parameters of SMA mixtures. Therefore, this study was conducted to determine the degree of aggregate degradation in SMA mixtures due to the compaction process. Aggregates of two Nominal Maximum Aggregates Sizes (NMAS), designated as SMA14 and SMA20, were compacted using 50 blows of the Marshall Hammer and 100 gyrations of the Superpave Gyratory Compactor (SGC). The verified samples were then prepared and extracted using the Centrifuge Method. The relationship between aggregate degradation and influencing factors, such as compaction effort and volumetric properties were investigated. Aggregate degradation by the Marshall Hammer was found to be significantly higher than degradation by the SGC. Voids in the mineral aggregate (VMA) of either compaction method decrease or are almost the same when aggregate degradation is not significant. SGC method can be selected to represent the field roller that results in a similar trend of aggregate degradation.

AB - Stone Mastic Asphalt (SMA) mixtures are designed to have a high coarse aggregate content and stone-on-stone contact, which results in more stress on the coarse aggregates during compaction and traffic loading. As a result, aggregates tend to break down more in SMA mixtures than in conventional dense graded mixtures. Aggregate degradation during compaction and traffic loading may cause changes in the original gradation and thus may also affect the volumetric parameters of SMA mixtures. Therefore, this study was conducted to determine the degree of aggregate degradation in SMA mixtures due to the compaction process. Aggregates of two Nominal Maximum Aggregates Sizes (NMAS), designated as SMA14 and SMA20, were compacted using 50 blows of the Marshall Hammer and 100 gyrations of the Superpave Gyratory Compactor (SGC). The verified samples were then prepared and extracted using the Centrifuge Method. The relationship between aggregate degradation and influencing factors, such as compaction effort and volumetric properties were investigated. Aggregate degradation by the Marshall Hammer was found to be significantly higher than degradation by the SGC. Voids in the mineral aggregate (VMA) of either compaction method decrease or are almost the same when aggregate degradation is not significant. SGC method can be selected to represent the field roller that results in a similar trend of aggregate degradation.

KW - Aggregate

KW - Compaction

KW - Degradation

KW - Gyratory

KW - Marshall

UR - http://www.scopus.com/inward/record.url?scp=84886449142&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=84886449142&partnerID=8YFLogxK

U2 - 10.11113/jt.v65.2155

DO - 10.11113/jt.v65.2155

M3 - Article

AN - SCOPUS:84886449142

VL - 65

SP - 111

EP - 114

JO - Jurnal Teknologi

JF - Jurnal Teknologi

SN - 0127-9696

IS - 3

ER -